Select a documented construction, not just a material name

The Dk entry for an HDI stackup should match the specified dielectric construction, frequency and measurement context. Start with the exact core or prepreg row, then check whether the number is intended for your electrical model. If the test method or material condition is missing, retain the row as a candidate and record the unresolved field before release.

This example shows how to read two rows from an original material table and turn them into a traceable modeling record. It supplements the Dk and Df modeling guide with a concrete selection exercise. HDI layer count alone cannot select a dielectric constant.

Read the row and the frequency column together

The table below uses two core constructions from page 2 of Isola’s I-Speed Dk/Df table, revision C, October 25, 2019. Both list 0.0050 inch (0.127 mm) thickness. They have different glass constructions and resin contents, and different Dk values at 10 GHz. This is a reading exercise using that identified revision, not confirmation of current stock or an approved material substitution.

Two selected core rows, with a review annotation added
FieldCandidate ACandidate B
Construction1 × 21162 × 1067
Resin content56.5%72.0%
Listed thickness0.127 mm0.127 mm
Dk at 10 GHz3.793.45
Df at 10 GHz0.00600.0059
Test-method field in this tableNot stated; request confirmationNot stated; request confirmation

Annotation: equal listed thickness does not make the rows electrically interchangeable. The table gives paired Dk/Df entries within each frequency column; copying the lower number as Dk would be a transcription error. Do not replace a missing method with an assumed IPC method borrowed from a different document.

Keep core and prepreg sections separate. A core row cannot silently define a build-up prepreg dielectric that happens to use similar glass. Identify the actual bonding construction and the finished dielectric separation with the fabricator; the prepreg resin-content guide explains the associated fill and thickness questions.

Keep a value attached to its evidence

Six fields needed beside a dielectric constant A complete dielectric input record contains the exact product and revision, physical construction, frequency, measurement method and axis, modeling purpose, and the approval state. Unknown method information remains visibly open. Dk input record 01 · Product / revisionTrace the source02 · ConstructionCore, glass, resin, ply03 · FrequencyKeep units explicit04 · Method / axisUnknown? Leave open05 · Model purposeImpedance, delay, loss06 · Review stateCandidate or accepted
Original documentation checklist. The six fields identify an input; they do not validate a material or replace electrical analysis.

A useful CAD note says more than “Dk = 3.79.” For the first row, a candidate record would identify I-Speed, core construction 1 × 2116, 56.5% resin, listed thickness 0.127 mm, 10 GHz, revision C, page 2, with method and model suitability awaiting confirmation. Keep the source date and retrieval date separate: downloading an older table today does not make it a new revision.

Distinguish a material test from a circuit design value

Rogers’ October 2021 overview of Dk/Df test methods distinguishes measurements of dielectric specimens from values extracted using fabricated circuits. It also explains that measurement direction matters: methods can sample the thickness direction or the plane of the material. Different results do not automatically mean one laboratory is wrong.

Rogers separately describes its circuit-oriented Design Dk and differential phase-length extraction in Managing PCB Materials Dielectric Constant Dk, September 11, 2018. That explanation does not establish that every number labeled Dk by another manufacturer uses the same definition.

Ask what the solver expects. Record whether copper roughness is handled independently or is represented in the supplied extraction/model. Avoid adding an unexplained Dk adjustment simply to force a simulation to match a measurement. First reconcile the finished geometry, copper model, reference planes and measurement setup.

Calculate the consequence of choosing the wrong row

As an original sensitivity exercise, hold a hypothetical line length at 100 mm and treat the entire dielectric as homogeneous, nonmagnetic, lossless and nondispersive. For an ideal TEM line, propagation delay is t = L√Dk / c, using c = 0.299792458 mm/ps. This deliberately simplified model isolates the Dk choice; it is not a measured I-Speed trace result.

Ideal 100 mm line: changing only the illustrative Dk input
InputCalculationDelay
Dk = 3.45100 × √3.45 / 0.299792458619.6 ps
Dk = 3.79100 × √3.79 / 0.299792458649.4 ps
Difference649.4 − 619.6, rounded29.8 ps, approximately 4.81% relative to the lower result

The two Dk inputs are alternative construction entries, not upper and lower manufacturing tolerances. The calculation therefore cannot establish a timing tolerance or predicted yield. It shows why a seemingly convenient row substitution deserves an electrical-model review.

For an outer-layer microstrip, some field energy is outside the laminate, so substituting the bulk Dk directly into this homogeneous-line equation is inappropriate. Real HDI channels also contain different dielectric regions, via transitions and frequency-dependent behavior. Use geometry and a suitable material model for those structures. The propagation-delay tool is useful for preliminary sensitivity checks when its assumptions match the question.

Resolve frequency and missing information before release

Select the column for the frequency being evaluated and preserve its units. A data rate is not, by itself, the frequency label to select from a table. For broadband channel work, request data or a supported model across the relevant band rather than treating one 10 GHz entry as constant at all frequencies. If interpolation is proposed, document the method and its limitations instead of concealing it in a spreadsheet cell.

  • Unmatched construction: request the actual glass, ply count and resin option; do not average adjacent rows to invent a material.
  • Unspecified method or axis: keep the model input provisional until the material supplier or fabricator provides the missing context.
  • Changed pressed thickness: update the geometry and check whether the approved electrical input still applies.
  • Material substitution: compare impedance, delay and loss assumptions separately, and record the approved replacement construction.

Use the material-selection tool to organize requirements, then retain the source row and open questions with the stackup. The release record should identify who owns each unresolved input and which revision was accepted.

Request a construction-specific material review

Send the exact material designation and table revision, selected core/prepreg rows, copper option, proposed finished thicknesses, layer stack, and the electrical or thermal requirements driving the choice. Mark uncertain Dk/Df inputs and the frequencies used in your model. These details make a material-review or quotation request actionable.

Send your material and stackup questions